1、GB/T23312.2-20097回弹性见GB/T23312.1一2009中第7章。8柔韧性和附若性见GB/T23312.1一2009中第8章。圆棒卷绕试验的圆棒直径应为2d。9热冲击见GB/T23312.1一2009中第9章。最小热冲击温度应为155C。10软化击穿试验要求正在考虑中,11耐刮(导体标称直径2.500mm及以下)漆包线耐刮性能应符合表1规定。表1耐刮1级2级导体标称直径最小平均每次试验中最小平均每次试验中mm刮破力最小刮破力刮破力最小刮破力NNNN0.4002.051.753.252.750.4502.201.753.502.950.5002.352.003.753.200.
2、5602.502.154.003.400.6302.702.304.303.650.7102.852.454.603.900.8003.052.604.954.200.9003.302.805.304.501.0003.553.005.654.801.1203.803.256.055.101.2504.103.506.455.501.4004.403.756.955.901.6004.754.007.456.301.800一8.006.752.0008.507.202.2409.107.702.500一9.708.20注:对于导体标称直径的中间尺寸,应取下一个较大导休标称直径的数值。12耐溶剂见GB/T23312.1一2009中第12章。