1、Designation:D151605(Reapproved 2010)Standard Test Method forWidth of Leather1This standard is issued under the fixed designation D1516;the number immediately following the designation indicates the year oforiginal adoption or,in the case of revision,the year of last revision.A number in parentheses

2、indicates the year of last reapproval.Asuperscript epsilon()indicates an editorial change since the last revision or reapproval.This standard has been approved for use by agencies of the Department of Defense.1.Scope1.1 This test method covers determination of the width ofphysical test specimens and

3、 of regularly shaped units andpieces of all types of leather.This test method does not applyto wet blue.1.2 The values stated in inch-pound units are to be regardedas standard.The values given in parentheses are mathematicalconversions to SI units that are provided for information onlyand are not co

4、nsidered standard.1.3 This standard does not purport to address all of thesafety concerns,if any,associated with its use.It is theresponsibility of the user of this standard to establish appro-priate safety and health practices and determine the applica-bility of regulatory limitations prior to use.

5、2.Referenced Documents2.1 ASTM Standards:2D1610 Practice for Conditioning Leather and Leather Prod-ucts for Testing3.Significance and Use3.1 This test method is designed to measure the width ofspecimens before and after they are subjected to various testswhich may change the width.A test procedure w

6、herein suchmeasurements could be used is the change in area of squarepieces when measuring the resistance of leather to syntheticperspiration solution.4.Apparatus4.1 Steel Scale,graduated to 0.02 in.(0.5 mm).4.2 Steel Tape,graduated to116in.or in millimetres.5.Specimen5.1 The specimen shall be the p

7、repared test specimen,unit,or piece.It shall be conditioned for 48 h in an atmospheremaintained at 73.4 6 1.8F(23 6 1C)and 50 6 4%relativehumidity and tested under these conditions.See PracticeD1610.6.Procedure6.1 Test SpecimensPlace the specimen on a flat surfaceand flatten it out without pulling o

8、r stretching.Measure thewidth to the nearest 0.02 in.(0.5 mm)at the locationsdesignated in the test method for making the particular test forwhich the specimen was prepared.7.Calculation and Report7.1 Report the width of the test specimens used as pre-scribed in the test method for making the partic

9、ular physicaltest for which the specimen was prepared.7.2 Report the average of the width measurements taken onany unit or piece to the same accuracy as observed on theoriginal measurements,as the width of the piece.8.Precision and Bias38.1 The following criteria may be used to judge the accept-abil

10、ity of results if at least 15 units have been tested.8.2 A coefficient of variation of 1.8%can be expectedbetween laboratories on specimens of headband leather sub-jected to a perspiration test.NOTE1The data used as a basis for this reproducibility statement wasobtained on a round robin with 3 labor

11、atories measuring width on thesame specimens.The specimens were 51 mm by 51 mm before theperspiration testing.8.3 BiasNo justifiable statement on bias can be madesince the true value of width of leather test specimens cannotbe established by an accepted reference method.9.Keywords9.1 area change;lea

12、ther;width1This test method is under the jurisdiction of ASTM Committee D31 on Leatherand is the direct responsibility of Subcommittee D31.07 on Physical Properties Thistest method has been developed in cooperation with theAmerican Leather ChemistsAssn.(Standard Method E5-1961).Current edition appro

13、ved Oct.1,2010.Published November 2010.Originallyapproved in 1957.Last previous edition approved in 2005 as D1516 05.DOI:10.1520/D1516-05R10.2For referenced ASTM standards,visit the ASTM website,www.astm.org,orcontact ASTM Customer Service at serviceastm.org.For Annual Book of ASTMStandards volume i

14、nformation,refer to the standards Document Summary page onthe ASTM website.3Supporting data for the reproducibility statement are filed at ASTM Headquar-ters and may be obtained by requesting Research Report RR:D31-1007.Copyright ASTM International,100 Barr Harbor Drive,PO Box C700,West Conshohocken

15、,PA 19428-2959.United States1 ASTM International takes no position respecting the validity of any patent rights asserted in connection with any item mentionedin this standard.Users of this standard are expressly advised that determination of the validity of any such patent rights,and the riskof infr

16、ingement of such rights,are entirely their own responsibility.This standard is subject to revision at any time by the responsible technical committee and must be reviewed every five years andif not revised,either reapproved or withdrawn.Your comments are invited either for revision of this standard or for additional standardsand should be addressed to ASTM International Headquarters.Your comments will receive careful consideration at a meeting of theresponsible technical committee,which you may

展开阅读全文
相关资源
猜你喜欢
相关搜索

当前位置:首页 > 专业资料 > 国外标准

copyright@ 2008-2023 wnwk.com网站版权所有

经营许可证编号:浙ICP备2024059924号-2