1、Designation:D100017Standard Test Methods forPressure-Sensitive Adhesive-Coated Tapes Used forElectrical and Electronic Applications1This standard is issued under the fixed designation D1000;the number immediately following the designation indicates the year oforiginal adoption or,in the case of revi

2、sion,the year of last revision.A number in parentheses indicates the year of last reapproval.Asuperscript epsilon()indicates an editorial change since the last revision or reapproval.This standard has been approved for use by agencies of the U.S.Department of Defense.1.Scope1.1 These test methods co

3、ver procedures for testingpressure-sensitive adhesive-coated tapes to be used as electri-cal insulation.These tapes are classified as follows:1.1.1 Class 1Non-elastomeric backings made from mate-rials such as:Paper,flat or creped,Fabric,uncoated or coated,Cellulose ester films,Polyethylene terephtha

4、late(polyester)films,Fluorocarbon polymer films,Composite filament films,Polyamide films,Polyimide films,andCombinations thereof.1.1.2 Class 2Elastomeric backings that are characterizedby both high stretch and substantial recovery.These backingsare made from materials such as:Vinyl chloride and co-p

5、olymers,Vinylidene chloride and co-polymers,andPolyethylene and co-polymers.1.2 Test laminates of Class 1 and Class 2 backings accord-ing to Class 1 test methods.1.3 The procedures appear in the sections indicated belowand in alphabetical order:Adhesion Strength to Steel and Backing at Room Temperat

6、ure46 53Adhesion Strength to Steel and Backing at Low Temperatures46 53Bond Strength After Solvent Immersion110 115Breaking Strength and Elongation at Room Temperature37 45Breaking Strength and Elongation at Low Temperatures37 45Conditioning6 8Curling and Twisting140 146Dielectric Breakdown Voltage8

7、3 90Effect of Accelerated Aging on High-Temperature Tapes97 103Flagging66 76Flammability104 109Hazards/Precautions3Insulation Resistance at High Humidity91 96Length of Tape in a Roll28 36Oil Resistance116 122Puncture Resistance123 128Resistance to Accelerated Aging(Heat and Moisture)129 139Sampling4

8、Specimen Preparation5Thermosetting Properties77 82Thickness21 27Unwind Force at Room Temperature54 65Unwind Force at Low Temperatures54 65Width11 20NOTE1These procedures apply to both Class 1 and Class 2 tapesexcept as noted above.1.4 This is a fire-test response standard(see Section 104).1.5 The va

9、lues stated in SI units are the standard,unlessotherwise noted.If a value for measurement is followed by avalue in inch-pound or English units in parentheses,it is likelythat the second value will only be approximate and it is forinformation only.The first stated value is the preferred unit.NOTE2The

10、se test methods are similar to IEC 604543,but may differsometimes in some details.1.6 This standard does not purport to address all of thesafety concerns,if any,associated with its use.It is theresponsibility of the user of this standard to establish appro-priate safety and health practices and dete

11、rmine the applica-bility of regulatory limitations prior to use.For specific hazardssee Section 3.1.7 This international standard was developed in accor-dance with internationally recognized principles on standard-ization established in the Decision on Principles for theDevelopment of International

12、Standards,Guides and Recom-mendations issued by the World Trade Organization TechnicalBarriers to Trade(TBT)Committee.2.Referenced Documents2.1 ASTM Standards:2A666 Specification for Annealed or Cold-Worked AusteniticStainless Steel Sheet,Strip,Plate,and Flat Bar1These test methods are under the jur

13、isdiction of ASTM Committee D09 onElectrical and Electronic Insulating Materials and are the direct responsibility ofSubcommittee D09.07 on Electrical Insulating Materials.Current edition approved July 1,2017.Published July 2017.Originally approvedin 1948.Last previous edition approved in 2010 as D1

14、000 10.DOI:10.1520/D1000-17.2For referenced ASTM standards,visit the ASTM website,www.astm.org,orcontact ASTM Customer Service at serviceastm.org.For Annual Book of ASTMStandards volume information,refer to the standards Document Summary page onthe ASTM website.Copyright ASTM International,100 Barr

15、Harbor Drive,PO Box C700,West Conshohocken,PA 19428-2959.United StatesThis international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for theDevelopment of International Standards,Guides and Recommendatio

16、ns issued by the World Trade Organization Technical Barriers to Trade(TBT)Committee.1 D149 Test Method for Dielectric Breakdown Voltage andDielectric Strength of Solid Electrical Insulating Materialsat Commercial Power FrequenciesD257 Test Methods for DC Resistance or Conductance ofInsulating MaterialsD295 Test Methods for Varnished Cotton Fabrics Used forElectrical InsulationD374/D374M Test Methods for Thickness of Solid Electri-cal InsulationD1711 Terminology Relating to Electrical InsulationD