1、Copyright by ASTM Intl(all rights reserved);Tue May 6 11:14:54 EDT 2014Downloaded/printed byRochester Institute Of Technology pursuant to License Agreement.No further reproductions authorized.STP 1309 Thermal and Mechanical Test Methods and Behavior of Continuous-Fiber Ceramic Composites Michael G.J

2、enkins,Edgar Lara-Curzio,Stephen T.Gonczy,Noel E.Ashbaugh,and Larry P.Zawada,Editors ASTM Publication Code Number(PCN):04-013090-30 ASTM 100 Barr Harbor Drive West Conshohocken,PA 19428-2959 Printed in the U.S.A.Copyright by ASTM Intl(all rights reserved);Tue May 6 11:14:54 EDT 2014Downloaded/printe

3、d byRochester Institute Of Technology pursuant to License Agreement.No further reproductions authorized.ISBN:0-8031-2033-8 PCN:04-013090-30 Copyright?9 1997 AMERICAN SOCIETY FOR TESTING AND MATERIALS,West Conshohocken,PA.All rights reserved.This material may not be reproduced or copied,in whole or i

4、n part,in any printed,mechanical,electronic,film,or other distribution and storage media,without the written consent of the publisher.Photocopy Rights Authorization to photocopy items for internal,personal,or educational classroom use,or the internal,personal,or educational classroom use of specific

5、 clients,is granted by the American Society for Testing and Materials(ASTM)provided that the appropriate fee is paid to the Copyright Clearance Center,222 Rosewood Dr.,Danvers,MA 01923;Tel:508-750-8400;online:http:/ Review Policy Each paper published in this volume was evaluated by two peer reviewer

6、s and at least one of the Editors.The authors addressed all of the reviewers comments to the satisfaction of both the technical editor(s)and the ASTM Committee on Publications.To make technical information available as quickly as possible,the peer-reviewed papers in this publication were prepared ca

7、mera-ready as submitted by the authors.The quality of the papers in this publication reflects not only the obvious efforts of the authors and the technical editor(s),but also the work of these peer reviewers.The ASTM Committee on Publications acknowledges with appreciation their dedication and contr

8、ibution of time and effort on behalf of ASTM.Printed in Philadelphia,PA March 1997 Copyright by ASTM Intl(all rights reserved);Tue May 6 11:14:54 EDT 2014Downloaded/printed byRochester Institute Of Technology pursuant to License Agreement.No further reproductions authorized.Foreword This publication

9、,Thermal and Mechanical Test Methods and Behavior of Continuous-Fiber Ceramic Composites,contains papers presented at the symposium of the same name held in Cocoa Beach,Florida on 8-9 Jan.1996.The symposium was sponsored by ASTM Committee C28 on Advanced Ceramics,ASTM Committee E08 on Fatigue and Fr

10、acture,and the American Ceramic Society,Engineering Ceramics Division.Michael G.Jenkins,University of Washington,Edgar Lara-Curzio,Oak Ridge National Laboratory,Stephen T.Gonczy,Gateway Materials Technology,Noel E.Ashbaugh,University of Dayton Research Institute,and Larry P.Zawada,Wright Laboratory,

11、presided as symposium cochairmen and are also the editors of the resulting publication.Copyright by ASTM Intl(all rights reserved);Tue May 6 11:14:54 EDT 2014Downloaded/printed byRochester Institute Of Technology pursuant to License Agreement.No further reproductions authorized.Contents Overview vii

12、 ROOM=TEMPERATURE TEST RESULTS/METHODS Influence of Test Mode,Test Rate,Specimen Geometry,and Bending on Tensile Mechanical Behavior of a Continuous Fiber Ceramic Composite-JOHN P.PICCOLA,JR.,MICHAEL G.JENKINS,AND EDGAR LARA-CURZIO Effect of High Strain Rate on the Tensile Behavior of NicalonrM/CAS

13、Continuous-Fiber Ceramic Composites-JOS M.SANCHEZ,IiqllGO PUENTE,REYES ELIZALDE,ANTONIO MARTIN,JOSE M.MARTNEZ,ADRIAN M.DANIEL,MANUEL FUENTES,AND COLIN P.BEESLEY Shear Strength of Continuous Fiber Ceramic Composites-EDGAR LARA-CURZIO AND MATTISON K.FERBER Unloading-Reloading Sequences and the Analysi

14、s of Mechanical Test Results for Continuous Fiber Ceramic CompositeS-MARC SrEEN AND JOSI-LORENZO VALLIS 16 31 49 HIGH-TEMPERATURE TEST RESULTSIVIETHODS The Effect of Hold Times on the Fatigue Behavior of an Oxide/Oxide Ceramic Matrix Composite-LARRY P.ZAWADA AND SHIN S.LEE Subcritical Crack Growth i

15、n Ceramic Composites at High Temperature Measured Using Digital Image Correlation-DANIEL R.MUMM,WINFRED L.MORRIS,MAHYAR S.DADKHAH,AND BRIAN N.COX Tensile and Fatigue Behavior of a Silicon Carbide/Silicon Carbide Composite at 1300 ONAL Stress-Temperature-Lifetime Response of Nicalon Fiber-Reinforced

16、Silicon Carbide(SIC)Composites in AirIHUA-TAY LIN AND PAUL F.BECHER Fatigue Crack Growth Behavior of a Woven HPZ/Silicon Carbide Ceramic Matrix CompositemviCTORIA A.KRAMB AND REJI JOHN Creep-Rupture Behavior of a Nicalon/SiC Composite-MICHAEL J.VERRILLI,ANTHONY M.CALOMINO,AND DAVID N.BREWER Retained Tensile Properties and Performance of an Oxide-Matrix Continuous-Fiber Ceramic Composite After Elevated-Temperature Exposure in Ambient Air-KURT L.MUNSON AND MICHAEL G.JENKINS 69 102 113 128 142 158